MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 6EF Extra-fine Grain Cemented Carbide for Rotary Tools  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK extra-fine grain cemented carbide grades have been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

The range of SANDVIK extra-fine grain cemented carbide grades have a tungsten carbide grain size of 0.6 µm. This grain size is precisely controlled to produce a tool material with an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

SANDVIK grade 6EF has been developed as a result of an extensive research program aimed at optimizing solid carbide tool performance in metal cutting applications.

6EF incorporates 6% cobalt (Co) and 94% tungsten carbide (WC). 6EF is recommended for solid carbide rotary tool applications in the ISO K05/K10 range. It has special advantages where high toughness, sharp edge profiles and exceptional wear resistance is required.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.85 g/cc0.5365 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 93.693.6
Hardness, Vickers 1850185030
Flexural Strength 3900 MPa566000 psiTransverse Rupture; ISO 3327
Compressive Strength 7400 MPa1.07e+6 psi
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 6.0 %6.0 %
WC 94 %94 %
 
Descriptive Properties
Corrosion Resistance, 1-104
Wear Resistance, 0-105

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik H10F Extra-fine Grain Cemented Carbide for Rotary Tools
Sandvik H6F Cemented Carbide for Can Tooling
Sandvik C6N 6% Nickel Binder Cemented Carbide, Seal Grade
Sapco Si.SiC Silicon Carbide
Sandvik DZ05 Extra-Fine Cemented Carbide for Metal Forming Applications

NSANDV031 / 18925

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.