MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
  • Interleave: LDPE
  • Side 1: Uncured Silicone Rubber
  • Substrate: Style 2113 Fiberglass
  • Side 2: Uncured Silicone Rubber
  • Interleave: LDPE

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milSide 1; Arlon SQA-TMS-003
 102 microns4.00 milSubstrate; Arlon SQA-TMS-003
 127 microns5.00 milSide 2; Arlon SQA-TMS-003
 305 microns12.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3636Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa900 psiSilicone Property; ASTM D412
Elongation at Break 550 %550 %Silicone Property; ASTM D412
Tear Strength 14.0 kN/m80.0 pliSilicone Property; ASTM D624
Peel Strength 2.56 kN/m14.6 pliBond Strength (S1 to S2); Arlon SQA-TMS-011
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 33.3 kV/mm845 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
Flammability Test 1.11.1Inches; Char Length; FAR 25.853 App F, Pt. 1, S. A1ii
 6.36.3Seconds; Flame and Glow Time; FAR 25.853 App F, Pt. 1, S. A1ii
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Post Cure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 21.1 °C
6.00 Month
@Temperature 70.0 °F
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)10.7Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARL9752 / 148905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.