MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Beijing Evergrow Resources BF-25 Basalt Needle Felt
Categories: Other Engineering Material; Composite Fibers

Material Notes: Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairing of engineering structure products.

    Advantages:
  • High strength
  • Incombustible
  • Good thermal properties
    • Good insulator
    • Will work at 500-800 degrees

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filament Diameter 9.0 - 13 µm9.0 - 13 µm
Thickness 23000 - 25000 microns906 - 984 mil
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0300 - 0.316 W/m-K0.208 - 2.19 BTU-in/hr-ft²-°Faccording to the difference density
 
Descriptive Properties
Flammability TestIncombustible
Length (m)10
Weight (g/m²)3750
Width (mm)1000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Aluminum, Al
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
Beijing Evergrow Resources BF-3 Basalt Needle Felt
DuPont™ Kevlar® 49 Aramid Fiber

PBEIJ046 / 90115

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.