MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound MFD03 Polypropylene, Unspecified (PP, Unspecified) (Europe)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP STAT-KON MFD03 compound is based on Polypropylene (PP) resin containing conductive carbon powder and 15% glass fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm0.0050 - 0.010 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 59.0 MPa8560 psi5 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi5 mm/min; ISO 527
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527
Elongation at Yield 2.4 %2.4 %5 mm/min; ISO 527
Tensile Modulus 4.30 GPa624 ksi1 mm/min; ISO 527
Flexural Strength 50.0 MPa7250 psibreak, 2mm/min; ISO 178
 88.0 MPa12800 psiyield, 2 mm/min; ISO 178
Flexural Modulus 4.10 GPa595 ksi2 mm/min; ISO 178
Flexural Strain at Break 3.7 %3.7 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 1.00e+6 ohm1000 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 134 µm/m-°C
@Temperature 23.0 - 60.0 °C
74.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 154 °C309 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 127 °C261 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 
Processing PropertiesMetricEnglishComments
Zone 2 215 - 225 °C419 - 437 °F
Zone 3 240 - 250 °C464 - 482 °F
Melt Temperature 225 - 250 °C437 - 482 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81325 / 289272

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.