MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RESPOL REPSOL PRIMEVA® P2430 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA copolymer REPSOL PRIMEVA® P2430 is recommended for injection molding as well as for blends with other products like waxes and mineral fillers. It contains antioxidant and free flowing agent.
Applications: Injection molding. Release agents containing silicone must be avoided; Blends with waxes; Manufacture of masterbatches; Microcellular foams; Extrusion of profiles and sheets with high flexibility
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant; Free Flowing Agent

Features: Antioxidant; Copolymer; Food Contact Acceptable; High Flexibility

Uses: Blending; Foam; Masterbatch; Profiles; Sheet

Agency Ratings: EU Food Contact

Processing Method: Extrusion; Foam Extrusion; Injection Molding; Profile Extrusion; Sheet Extrusion

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ISO 1183
Brookfield Viscosity  3.728e+6 cP
@Temperature 180 °C
3.728e+6 cP
@Temperature 356 °F
Spindle SC4-27
 6.696e+6 cP
@Temperature 200 °C
6.696e+6 cP
@Temperature 392 °F
Spindle SC4-27
Vinyl Acetate Content 24 %24 %
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979ISO 868
Hardness, Shore D 2929ISO 868
Tensile Strength at Break 25.0 MPa3630 psiISO 527-2
Elongation at Break 740 %740 %ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 77.2 °C171 °F
Ring & Ball Softening Point 162 °C324 °FASTM E28
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1323 / 312016

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.