MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Endex™ 160 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: A water-white thermoplastic resin made from purified aromatic hydrocarbon monomers. Used to modify the melt flow and increase the temperature resistance of styrenic plastic and rubber. Reinforces the styrene end blocks of styrenic block copolymers. In adhesives Endex™ 160 hydrocarbon resin will associate with the styrenic endblocks, producing higher cohesion at temperatures up to 70°C without affecting tack and adhesion properties. Endex™ 160 hydrocarbon resin has the highest softening point among all hydrocarbon resins available from Eastman Chemical Company.

Application/Uses:

  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Tapes and Labels
Key Attributes:
  • Heat stability
  • Highest softening point available
  • Pure aromatic monomer composition
  • Water-white initial color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  1000 cP
@Temperature 245 °C
1000 cP
@Temperature 473 °F
Melt
 10000 cP
@Temperature 210 °C
10000 cP
@Temperature 410 °F
Melt
 100000 cP
@Temperature 180 °C
100000 cP
@Temperature 356 °F
Melt
Molecular Weight 2900 g/mol2900 g/molMz
 9200 g/mol9200 g/molMw. Mw/Mn ratio = 3.6
 22500 g/mol22500 g/molMn
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 110 °C230 °F
Ring & Ball Softening Point 158 °C316 °FASTM E 28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point-12°CDACP
 152°COMS
 16°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5319 / 222513

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.