System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Axiall 22950 Coax & Telecom Flexible PVC
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
Material Notes:
Riser jacket, 25 mil over HDPE primaries.
Information provided by Georgia Gulf
Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.48
-
1.52
g/cc
1.48
-
1.52
g/cc
ASTM D-792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
92 - 98
92 - 98
delayed; ASTM D-2240
Tensile Strength, Yield
18.6
MPa
2700
psi
ASTM D-638
Elongation at Yield
310 %
310 %
ASTM D-638
100% Modulus
13.8
MPa
@Strain 100 %
2000
psi
@Strain 100 %
ASTM D-638
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-16.0
°C
3.20
°F
ASTM D-746
Oxygen Index
36 %
36 %
ASTM D-638
Processing Properties
Metric
English
Comments
Melt Temperature
191
°C
375
°F
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
RTP Company RTP 2999 X 125934 A NS Polyether-Block-Amide (PEBA / COPA); Barium Sulfate Filled
LyondellBasell Hostacom ERC 198N G31325 Polypropylene Copolymer, 18% Talc Filled
LyondellBasell Hifax TRC 135X/4 C12823 Polypropylene with 20% Talc
LyondellBasell Dexflex 911-UV Thermoplastic Polyolefin, 10% Talc Filled
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene
PGGUL045 / 41321
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.