MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M ScotchPad™ 818CP Custom Printed Marking Tapes
Categories: Polymer; Adhesive

Material Notes: 3M™ ScotchPad™ Custom Printed Marking Taps 818CP are individual paper tags laminated to the strongest conformable backing and most consistent pressure-sensitive hot-melt adhesive system available. These tags have adhesive below one short edge for strong attachment to many surfaces. The protective, strong 3M™ Scotchpro™ Polypropylene top surface allows clear reading of the printed material but shields the print from abrasion, dirt, liquids. These tags are stacked 25 to a pad with a backsheet. The tags can be placed on flat surfaces or wrapped around thinner objects. When the adhesive is placed against the tag’s back paper surface, the paper will tear upon removal and provide tamper evidence.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 78.7 microns3.10 milTape; ASTM D3652
 81.3 microns3.20 milPaper; ASTM D3652
 155 microns6.10 milTab; ASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 7.57 MPa1100 psiLongitudinal; ASTM D3759
 15.1 MPa2200 psiTransverse; ASTM D3759
Elongation at Break 160 %160 %ASTM D3759
Peel Strength 0.60259 kN/m3.4375 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypePressure sensitive synthetic rubber resin
AppearanceBlue, red, white yellow, or custom

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34145 / 168892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.