MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

The Chemical Company DICYANDIAMIDE, C2H4N4
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Commonly known as DICYandiamide (DICY), the white crystalline compound is the dimer for cyanamide or for cyanoguanidine. The primary use of the chemical is in the production of melamine, but it is also as a curing agent for epoxy resins. DICY crystals melt at 45° C, and are soluble in water and alcohol. Other uses for the compound are in the manufacture of fertilizers, explosives, oil well drilling muds, pharmaceuticals, and dyestuffs.
Handling Instructions:Store in a cool, dry, well ventilated warehouse, and keep away from moisture.
Molecular Formula: C2H4N4

Information provided by The Chemical Company

Key Words: Cyanoguanidine;DICY;CAS Number 461-58-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 48 Mesh48 Mesh= 40% particles larger
Ash <= 0.050 %<= 0.050 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 209 - 211 °C408 - 412 °F
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca 0.020 %0.020 %
 
Descriptive Properties
AppearanceWhite Crystals
Assay= 99.5%
Impurity Precipitating TestAcceptable
Weight Loss (%)= 0.3%dry loss

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTCC006 / 106995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.