MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Parson Adhesives SONLOCK™ 3272 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive

Material Notes: SONLOK 3272 is a fast curing, high strength, high temperature resistance anaerobic thread locking compound for sealing and locking of studs, nuts, screws, bolts and fittings. SONLOK 3272 is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals.

Applications:

  • Ideal for applications where the temperatures range up to 200°C.
  • Ideal for thread locking heavy duty applications such as bolts used in transmission, construction equipment or railroad assemblies, etc.
  • Lubricated for easy assembly. Prevents loosening and leakage of threaded fasteners. Locks and seals threaded joints-nuts, screws, and studs.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Brookfield Viscosity 9500 cP9500 cPRVT, Spindle 3 @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 14.49 MPa2102 psiSteel Pins & Collars; ISO 10123
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point >= 93.0 °C>= 199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling
 60.0 - 180 min1.00 - 3.00 hourFunctional
 1440 min24.0 hourFull
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorRed
CompositionMethacrylate Ester
Initial Strength Retained (%)100Gasoline for 500 hrs at 22°C
 100Gasoline for 1000 hrs at 22°C
 100Break Fluid for 500 hrs at 22°C
 100Break Fluid for 1000 hrs at 22°C
 100Ethanol for 500 hrs at 22°C
 100Ethanol for 1000 hrs at 22°C
 85Water/Glycol for 1000 hrs at 87°C
 90Water/Glycol for 500 hrs at 87°C
 95Acetone for 500 hrs at 22°C
 95Acetone for 1000 hrs at 22°C
 95Motor Oil for 500 hrs at 125°C
 95Motor Oil for 1000 hrs at 125°C
Solvent ContentNone
Torque23 NmBreakaway, M10 steel nuts and bolts, ISO 10964
 25 NmPrevail, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN021 / 186464

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.