MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo PULSE™ 840P ABS + Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin has been used in automotive instrument panel and interior trim applications.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM Data
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/in
Melt Flow 2.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 48.3 MPa7010 psiASTM Data
Tensile Strength, Yield 51.7 MPa7500 psiASTM Data
Elongation at Break 100 %100 %ASTM Data
Elongation at Yield 4.8 %4.8 %ISO Data
Tensile Modulus 2.10 GPa305 ksiISO Data.
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inASTM Data
 5.34 J/cm
@Temperature -50.0 °C
10.0 ft-lb/in
@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NBNBISO Data, Low Temp
 NBNBISO Data
Charpy Impact, Notched 2.40 J/cm²11.4 ft-lb/in²ISO Data, Low Temp
 6.10 J/cm²29.0 ft-lb/in²ISO Data
Instrumented Impact Total Energy  50.9 J
@Temperature -30.0 °C
37.5 ft-lb
@Temperature -22.0 °F
 50.9 J
@Temperature 23.0 °C
37.5 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °FUnannealed; ASTM Data

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® NH-1033 PC/ABS
Lotte Advanced Materials Infino® LX-1098F PC/ABS
Lotte Advanced Materials Infino® HP-1000XB PC/ABS
Lotte Advanced Materials Infino® HP-1000P PC/ABS, Unreinforced
Lotte Advanced Materials Infino® HP-1000H PC/ABS, Unreinforced

PZZDW130 / 34361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.