MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Smooth-Cast® 325 Ultra Low Viscosity Liquid Plastics
Categories: Polymer; Thermoplastic

Material Notes: Product Overview: The Smooth-Cast™ 325, 326 & 327 ColorMatch™ Series plastics are fast-cast resins that were developed specifically for adding color pigments and fillers to achieve true color representation or filler effect. The ColorMatch™ Series is formulated “color neutral”. Small amounts of pigment will yield accurate, vivid colors from cured castings using So-Strong™, UVO™ or Ignite™ colorants. The ColorMatch™ Series offers the convenience of a 1A: 1B mix ratio by volume and has a very low viscosity. Demold times range from about 10 minutes to 2-4 hours (depending on product, mass and mold configuration). Note: Large mass castings will get very hot and shrink more, depending on mold configuration. The ColorMatch™ Series also readily accept fillers (such as URE-FIL™ 3 from Smooth-On). Because of its neutral color, Smooth-Cast™ 325 is ideal for creating marble and wood grain casting effects, or duplicating the look of real metal by adding bronze, brass or other metal powder. Applications for the ColorMatch™ Series plastics include making pigmented prototype models or figures, special effect props, reproducing small to medium size sculptures, decorative jewelry, etc.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D-1475
Viscosity 100 cP100 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D-2240
Tensile Strength, Ultimate 21.9 MPa3170 psiASTM D-638
Elongation at Break 10 %10 %ASTM D-638
Tensile Modulus 0.965 GPa140 ksiASTM D-638
Flexural Strength 25.4 MPa3690 psiASTM D-790
Flexural Modulus 0.696 GPa101 ksiASTM D-790
Compressive Strength 24.1 MPa3500 psiASTM D-695
Compressive Modulus 0.252 GPa36.5 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 50.0 °C122 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling Time
Pot Life 2.50 min2.50 minASTM D-2471
 
Descriptive Properties
ColorClear Amber
Mix Ratio115A:100Bby weight
 1A:1Bby volume
Specific Volume25.9[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN022 / 296723

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.