Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
INEOS Styrolution Luran® HD-20 SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very good transparency and a light intrinsic color.
  • Compliant with USP Class VI and ISO 10993-5
  • Excellent transparency
  • Good surface appearance
  • Good chemical resistance
  • Resistant to beta and gamma sterilization

Information provided by Styrolution

Key Words: HD 20
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage 0.0030 - 0.0070 in/inISO 294-4
Melt Flow 22 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83
Ball Indentation Hardness 165 MPaISO 2039-1
Tensile Strength, Yield 72.0 MPaISO 527
Elongation at Yield 3.0 %ISO 527
Tensile Modulus 3700 MPaISO 527
Flexural Strength 120 MPaISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
 2.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
Charpy Impact Unnotched 16.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 2.00 kJ/m²ISO 179
Tensile Creep Modulus, 1 hour 3500 MPaISO 899
Tensile Creep Modulus, 1000 hours 2800 MPaISO 899
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0040
@Frequency 100 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CISO 11359
Thermal Conductivity 0.170 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °CISO 75
Vicat Softening Point 106 °C
@Load 5.10 kg
50°C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.569
@Wavelength 589.3 nm
Sodium D Line; ASTM D 542
Transmission, Visible >= 89 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CISO 294
Mold Temperature 50.0 °CISO 294
Injection Velocity 200 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Tyril® 100 SAN
Dow Tyril® 125 SAN
INEOS Styrolution Absolan® 2150 SAN
Chi Mei Kibisan® PN-117C SAN
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)

PBASF8022 / 159704

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.