MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Phillips 66 100 Ultra-Clean Super Hydraulic Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 14/11. Careful attention to particle control leads to high cleanliness fluids appropriate for use in critical applications. Ultra-Clean Super Hydraulic Oils are recommended for use in a variety of high-pressure mobile and stationary hydraulic systems utilizing vane, piston or gear pumps, especially where particle contamination can create operational problems. By virtue of their composition, Ultra-Clean Super Hydraulic Oils have the same performance rating and meet the same approval criteria as Super Hydraulic Oils, thus meeting Denison Hydraulics' HF-0 requirements and Cincinnati Machine's P-68 (ISO 32), P-70 (46) and P-69 (68) specifications. Similarly, Ultra-Clean Super Hydraulic Oil exceeds Vickers M-2950-S, Vickers I-286-S and U.S. Steel 127 and 136 requirements. Ultra-Clean Super Hydraulic Oils are available in ISO Viscosity Grades 32, 46, 68 and 100.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Viscosity Measurement 9898Viscosity Index
Saybolt Viscosity at 100°F 522 SUS522 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt100 cSt
Kinematic Viscosity at 100°C (212°F) 11.2 cSt11.2 cSt
Oxidative Stability 4500 hour4500 hourASTM D 943
ASTM Color 0.500.50
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.450 mm0.0177 in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm889 kV/inNo thickness given
 
Thermal PropertiesMetricEnglishComments
Pour Point -31.7 °C-25.0 °F
Flash Point 249 °C480 °F
 
Descriptive Properties
Emulsion Characteristics (40-40-0)10 minutes
FZGPass 10 Stages
ISO Cleanliness Code14/11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON197 / 75234

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.