A cross linker used as an additive to Ultra chrome 452 when there is a requirement for increased adhesion. This would typically arise when the Ultra chrome 452 is being applied onto old 5410 or there is a time delay in production between Ultra thane 5410 and Ultra chrome 452 over coating. RECOMMENDED APPLICATIONS: Only to be used with Ultra chrome 452. FEATURES: • Specifically for use with Ultra chrome 452 as a cross linker to increase adhesion. Information provided by ITW Performance Polymers. |