SCG HDPE H568JA is a high density polyethylene resin with excellent environment stress cracking resistance and good mechanical properties balance. It is particularly designed for light-weight carbonated soft drink caps. This resin have excellent process ability for both injection and continuous compression molding. Related Finished Products: Caps and closures for carbonated soft drinks and hot fill beverages. Applications: Beverage caps and closures (carbonated soft drink, sparkling water). Features: Excellent process ability. Excellent environmental stress cracking resistance. Good mechanical property. Good organoleptic property. Information provided by SCG. |