MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultradur® B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³ISO 1183
Viscosity Number 75 cm³/g0.75 dl/g
Melt Flow 110 g/10 min
@Load 10.0 kg,
Temperature 275 °C
110 g/10 min
@Load 22.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 170 MPa24700 psi5mm/min; ISO 527
Elongation at Break 1.4 %1.4 %5mm/min; ISO 527
Tensile Modulus 18.7 GPa2710 ksi1mm/min; ISO 527
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO 179
 6.40 J/cm²
@Temperature -30.0 °C
30.5 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °F10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75
 
Descriptive Properties
ColorBK15029
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
BASF Ultradur® B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET
BASF Ultradur® B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
BASF Ultradur® B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET

PBASF9060 / 84824

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.