MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) CAF® 730 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 730 is a one component, thixotropic silicone elastomer, which cures at room temperature simply on contact with air humidity. It is a product that is :
  • Non flowing.
  • High extrusion.
  • Multi-purpose.
Applications: CAF 730 is particularly suited to bonding, protection and maintenance applications. It is recommended for :
  • Bonding/sealing in the aeronautics industry.
  • Elastic bonding or protection of electronic components.
  • Flexible bonding/bonding between metal and/or plastic components.
  • Repair/servicing in industry and transport applications
Advantages:
  • Non corrosive.
  • Low odour.
  • Excellent thermal ageing.
  • Good dielectric properties.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccISO R 1183
 1.03 g/ccafter curing; ASTM D297
Storage Temperature 2.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25ASTM D2240
Tensile Strength 276 psiASTM D412
Elongation at Break 400 %ASTM D412
Shear Strength 0.200 MPaon Alu AG3, primerless, joint 1 mm thick, adhesive failure
 1.00 MPaon polyesters, polyamides, ABS, polycarbonate, PMMA with PM 820, joint 1 mm thick, 100% cohesive failure
 1.20 MPaon Alu AG3 or on stainless steel with primer PM 820, joint 1 mm thick, 100% cohesive failure
Tear Strength 22.8 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+15 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 483 V/milASTM D419
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.260 W/m-K
Maximum Service Temperature, Air 200 °C
@Thickness 2.00 mm,
Time 3.60e+6 sec
 225 °C
@Thickness 2.00 mm,
Time 259000 sec
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Extrusion Rate >= 120 g/min3mm, 3bars, norm 495A
Cure Time 7.00 minSkin formation
 7.00 hour
@Thickness 2.00 mm
 24.0 hour
@Thickness 4.60 mm
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancenon flowing paste
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) CAF® 7037 Silicone Rubber
Overview of materials for Silicone Rubber
Overview of materials for Acrylic, Cast
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Elkem (Bluestar Silicones) CAF® 4 Silicone Rubber

PBLUST095 / 191071

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.