MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Categories: Metal

Material Notes: Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut Gaskets

Available Forms: Die-Cut Elastomer with Joined EMI Strips.

Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  20 - 30 dB
@Frequency 14000 Hz
20 - 30 dB
@Frequency 14000 Hz
 83 - 93 dB
@Frequency 1e+9 Hz
83 - 93 dB
@Frequency 1e+9 Hz
 >= 102 dB
@Frequency 1.80e+7 Hz
>= 102 dB
@Frequency 1.80e+7 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °FNeoprene Version
 204 °C399 °FSilicone Version
Minimum Service Temperature, Air -62.0 °C-79.6 °FSilicone Version
 -34.0 °C-29.2 °FNeoprene Version
 
Descriptive Properties
Maximum Joint Unevenness, % of Gasket Height0.25Class C- Completely Interchangeable
 0.3Class A- Permanently Closed
 0.3Class B- Open-Close in Same Position

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 K8 9 FR grey (3840) PA6 FR, Dry, 20% Glass Filled
Mitsubishi Chemical Advanced Materials Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet)
Hexcel® HexWeb® CR III 5/32-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Thermal Ceramics Kaowool Blanket, Blanket S Mesh Enclosed Rounds, Strips and Blankets

PCHOME293 / 131003

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.