MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Pro-fax RP223L Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Pro-fax RP223L is a medium melt flow rate polypropylene random copolymer available in pellet form. This resin is typically used in cast and oriented film applications. In film applications it offers exceptional clarity, gloss, improved cold temperature impact resistance and lower and broader heat sealing properties as compared to conventional polypropylene homopolymer. Pro-fax RP223L is a barefoot resin with no slip, anti-block or other property specific additives. This product is manufactured with a non-phthalate catalyst system and is produced without animal derived components.

Availability: North America

Application: Bags & Pouches; Breathable Film; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Hygiene Film; Stationery Film; Twist Wrap Film

Processing Method: Cast Film; Oriented Film

Attribute: Good Heat Seal; Good Optical Properties; Good Processability; Medium Flow

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 7.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.2 MPa3800 psi50 mm/min; ASTM D638
Elongation at Yield 13.0 %13.0 %ASTM D638
Flexural Modulus 0.896 GPa130 ksi1.3 mm/min, 1% Secant, Procedure A; ASTM D790
Izod Impact, Notched 0.510 J/cm0.955 ft-lb/inMethod A; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9771 / 324706

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.