Nucleated, excellent sidewall stiffness and heat resistance. Produced without animal derived components Processing: Typical processing temperature range of 450 to 500°F (232-260°C) Applications: Portion cups, hot and cold beverage lids, and food containers Regulatory: FDA – 21 CFR 177.1520(c) 1.1a; USP <88> Class VI Information provided by INVISTA. |