MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Hifax™ CB189FC Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low fogging

Applications: automotive instrument panel components, knee bolsters and end caps, glove box doors

Description: Hifax CB189FC medium melt flow, minearl-filled thermoplasstic olefin resin has a very good balance of impact, stiffness, dimensional stability and processability. It was designed specifically for use in various automotive interior trim components.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inTool, Montell
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 18.0 MPa2610 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus, 1% Secant 1200 MPa174000 psi0.05 in/min; ASTM D790A
Izod Impact, Notched 6.40 J/cm12.0 ft-lb/inASTM D256A
Gardner Impact 25.0 J18.4 ft-lbASTM D3029
 19.0 J
@Temperature -30.0 °C
14.0 ft-lb
@Temperature -22.0 °F
ASTM D3029
Instrumented Impact Energy at Peak 15.0 J
@Temperature -30.0 °C
11.1 ft-lb
@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C180 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMO450 / 53639

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.