MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger DELRIN® 100AF natural blend POM-H, PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes:
  • excellent wear properties
  • low static friction
  • high mechanical load capacity
  • good machinability
Target Industries:
  • conveyor technology
  • automotive industry
  • business machines
  • heavy duty industry
  • printing machines
  • packaging and paper machinery

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.50 g/cc
Moisture Absorption 0.120 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 79ASTM D 785
Tensile Strength, Yield 8100 psiASTM D 638
Elongation at Break 10.3 %ASTM D 638
Modulus of Elasticity 310 ksiASTM D 638
Flexural Strength 12700 psiASTM D 790
Flexural Modulus 485000 psiASTM D 790
Compressive Yield Strength 12500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 1200 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 250000 psiASTM D 695
 
Thermal PropertiesOriginal ValueComments
Melting Point 347 °FDIN EN ISO 11357
Maximum Service Temperature, Air 185 °FLong Term
 300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 334 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 244 °FASTM D 648
 
Descriptive Properties
Colorbrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8133 / 319061

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.