MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Specialty Materials Hy-Bor 208 Boron/Graphite Hybrid Prepreg Tape
Categories: Polymer; Thermoset; Epoxy

Material Notes: Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil boron fibers, Hy-Bor material can be manufactured to incorporate any commercially available graphite prepreg. By altering the spacing of the boron fiber in the prepreg, performance properties and material costs can be tailored to meet the needs of a variety of demanding applications.

Property data reported for 208 filaments/inch 4-mil boron fiber with MR-40 carbon fiber and NCT-301 resin system.

Information provided by Specialty Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.97 g/cc0.0712 lb/in³
Thickness 165 microns6.50 milcured ply
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1900 MPa276000 psi
Elongation at Yield 0.80 %0.80 %
Modulus of Elasticity 240 GPa34800 ksi
Flexural Yield Strength 2410 MPa350000 psi
Flexural Modulus 215 GPa31200 ksi
Compressive Yield Strength 2760 MPa400000 psi
Compressive Modulus 240 GPa34800 ksi
Shear Strength 90.0 MPa13100 psiShort Beam
 103 MPa14900 psiInterlaminar
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 121 °C250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Specialty Materials 5521 Boron Epoxy Prepreg Tape
DuPont™ Kevlar® 49 Aramid Fiber
Zoltek™ PX35 Carbon Fiber Prepreg Tape
Goodfellow Polyaramid/Vinylester Composite Tube or Rod
DSM Dyneema® Max Technology

PSPEC02 / 68531

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.