MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BCF 30 X H2.0 901510 Nylon 6 (PA6), 30% Glass/Carbon Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PA 6, 30% glass fibers/carbon fibers, injection molding, heat-aging stabilized, improved electrical conductivity

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.334 g/cc0.04819 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0015 cm/cm0.0015 in/in150x105x3; 280 °C / MT 80°C; 500 bar; ISO 294-4
 0.0022 cm/cm0.0022 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0075 cm/cm0.0075 in/in150x105x3; 280 °C / MT 80°C; 500 bar; ISO 294-4
 0.0077 cm/cm0.0077 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi5 mm/min; ISO 527-1,-2
Elongation at Break 5.0 %5.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 6.70 GPa972 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 160 MPa23200 psi2 mm/min; ISO 178-A
Flexural Yield Strength 145 MPa
@Strain 3.5 %
21000 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 6.80 GPa986 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 5.0 %5.0 %2 mm/min; ISO 178-A
Izod Impact, Unnotched (ISO)  60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Puncture Energy  1.70 J
@Temperature -30.0 °C
1.25 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 2.40 J
@Temperature 23.0 °C
1.77 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min (Dry); ISO 11357-1,-3
Shrinkage, MD  0.030 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.030 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
 0.030 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.030 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD  0.080 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.080 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding
 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 120 °C176 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BCF 30 X H2.0 901510 Nylon 6 (PA6), 30% Glass/Carbon Fiber Reinforced, Dry
Celanese Zytel® 70G35HSLRA4 BK267 PA66-GF35
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3WG7 35% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3WG6 30% Glass Filled PA66 (Dry)

PLANW9295 / 208102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.