MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation properties, along with elevated temperature resistance. It has a forgiving one to one mix ratio by weight or volume. Although the system cures at room temperature, its physical properties are optimized by a post cure at 150°F for 2-3 hours. EP21ANHT adheres well to a wide variety of substrates including metals glass and many plastics. Its tensile shear strength exceeds 1,100 psi, enabling it to be used in many applications where high strength bonds are required. Other features include superior dimensional stability and a long working life. EP21ANHT offers good resistance to a wide range of chemicals including water, oil, fuels, and various solvents over the temperature range of -60°F to +400°F. The color of Part A is light gray; Part B is gray in color. EP21ANHT is widely used in electronic, electrooptical and related industries where excellent heat transfer and electrical insulation are required.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio.
  • Long working life.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly.
  • Low coefficient of expansion, low shrinkage, superb dimensional stability.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required.
  • High bonding strength to a wide variety of substrates.
  • Good durability, thermal shock and chemical resistance.
  • Great thermal conductivity; excellent electrical insulation properties.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 50000 - 110000 cPPart B
 200000 - 600000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 85
Tensile Strength at Break 5000 psi
@Temperature 23.9 °C
Tensile Modulus >= 500000 psi
@Temperature 23.9 °C
Shear Strength >= 1100 psiAl/Al, tensile
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 4.9
@Frequency 60 Hz,
Temperature 25.0 °C
Dielectric Strength >= 400 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 - 25.0 µm/m-°C
Thermal Conductivity 22.0 - 24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 48.0 - 72.0 hour
@Temperature 23.9 °C
Pot Life >= 90 min100 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
in original, unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21NDFG Two component epoxy compound for high performance applications
Master Bond EP21SC-1 Two Component Epoxy Resin System
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system
Master Bond EP21AOLV-2LO Two Part, Thermally Conductive and Electrically Insulative Epoxy

PMASTB306 / 149553

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.