LORD Thermoset 7195-125 Black adhesive is a one-component epoxy adhesive designed for use in SMD component mounting where non-stringing is necessary. Features: provides excellent thermal stability. rapidly cures at 121°C and 177°C. thixotropic rheology allows shape to be maintained after dispensing. provides excellent resistance to acids and strong bases. All information provided by Lord. |