MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.

Information supplied by Sumitomo Bakelite North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.800 g/ccPowder; ASTM D1895
Density 1.82 g/ccASTM D-792
Water Absorption 0.10 %48 hour; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 55.0 MPaASTM D638
Flexural Strength 79.0 MPaASTM D790
Flexural Modulus 13.8 GPaASTM D790
Compressive Strength 207 MPaASTM D695
Izod Impact, Notched 0.290 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 13.7 kV/mmST; ASTM D149
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 282 °CPost Baked; ASTM D648A
 
Descriptive Properties
Available Molding GradesCompression, Transfer, Injection
ColorBlack
FormGranular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® X22 Phenolic Formaldehyde Resin, UL Listed
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac

P90XR14 / 21228

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.