Polymerization System: Cold emulsion Polymerization Emulsifier: Rosin Acid Soap Stabilizer: Staining Coagulant: Acid Characteristics: Better physical properties than its corresponding hot rubber, excellent tack properties and good wear and flexing resistance Application: Tire, camelback, conveyor belt, rubber sheets or clothes as well as molded or extruded mechanical goods. Test Recipe, ASTM D-3185 Parts Taipol SBR-1500E - 100.00 Zinc oxide - 3.00 Stearic acid - 1.00 Sulfur - 1.75 HAF black(IRB#9) - 50.00 TBBS - 1.00 Total - 156.75 Information provided by TSRC Corporation |