MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Rike Chemical HELI™ HLC-3235 PVC Impact Modifier-CPE Series
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: The weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger intermolecular force, when PVC products are impacted, the relative displacement between PVC molecules is hard to take place, thus impact energy can not be effectively transferred into internal friction heat, resulting in the breaking of PVC materials. But owing to higher glass temperature and worse dispersibility of CPE, thus low temperature impact strength of CPE is not ideal. Moreover, due to heat stabilizers in PVC blend can not permeate into CPE, therefore CPE which is filled in PVC compound is easy to decompose, so that the heat stability of PVC products modified by CPE is very worse. Thus, the key questions to improve the PVC impact strength is how to largely reduce the PVC intermolecular force and so that increasing the speed that the PVC impact energy transfers into the heat energy.

Properties: Higher impact strength, good flexibility

Applications: PVC profile, PVC pipe

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.40 %
Particle Size 900 µm<2%
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 23 - 27 %
 
Descriptive Properties
AppearanceWhite powder
Colored Particles (Pcs/100g)<60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE-37-11 RoHS Black Polyethylene, Chlorinated (CPE)
Aurora Plastics TufGuard E™ CPE 12-020 CPE, Flame Retardant
BorsodChem ONGRO CPE 4002 N Chlorinated Polyethylene
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene

PSHAN081 / 103471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.