MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem Lowilite™ UV B1260 Antioxidant & Stabilizer
Categories: Other Engineering Material

Material Notes: Product Description: Lowlite™ UV B1260 stabilizer is a highly effective liquid blend of polymer stabilizers, with special emphasis on protection of polyurethanes against exterior weathering.

Application: Lowlite™ UV B1260 stabilizer was developed specifically to protect polyurethanes exposed to exterior weathering conditions. Applications include outdoor integral skin applications, shoe soles, window sealants etc. Lowlite™ UV B1260 is a combination of both thermal and UV-stabilizers and being a low viscosity liquid blend, soluble in all commonly used polyols, it is easy to pump and does. Lowlite™ UV B1260 is also very suitable for light stable prolyurethane-based pastes.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
Brookfield Viscosity 50 cP
@Temperature 60.0 °C
measured @ 20-100 rpm
 160 cP
@Temperature 40.0 °C
measured @ 20-100 rpm
 375 cP
@Temperature 30.0 °C
measured @ 20-100 rpm
 600 cP
@Temperature 25.0 °C
measured @ 20-100 rpm
 
Thermal PropertiesOriginal ValueComments
Pour Point 32.0 °F
 
Descriptive Properties
AppearanceYellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH498 / 315416

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.