MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Guang Dong LH-PS96 Conductive PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Application Field: Suitable for extrusion IC carrier tape, conductive sheet, blister packing box, which can be used in plastic packaging products

Feature: Low water absorption rate, good thermal stability, good toughness, high impact and good liquidity, dimensional stability

Grade: Extrusion Grade

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 - 1.14 g/ccGB/T1033
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
GB/T3682
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.7 MPaGB/T1040-1992
Flexural Strength 42.26 MPaGB/T9341-2008
Flexural Modulus 2485.03 MPaGB/T9341-2008
Tensile Impact Strength 2.843 kJ/m²GB/T1843-80
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohm - 1e+05GB/T1410

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGDON019 / 283967

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.