MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem FeSi 0.50 Al Low Al Ferrosilicon
Categories: Metal

Material Notes: Low Al Ferrosilicon compared to regular ferrosilicon will lower the content of aluminum inclusions in the final steel. In high carbon steels use of low Al FeSi will assist in the prevention of nozzle blockage during continuous casting. Reduced amounts of aluminum inclusions will help to avoid surface defects, particularly relevant to mirror finish stainless steel. For the production of tire cord, in which inclusion control is also important, manufacturer recommends the use of High Purity Ferrosilicon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 1.60 g/cc>= 0.0578 lb/in³
Density 3.20 g/cc0.116 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
Particle Size 3000 - 50000 µm3000 - 50000 µm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1100 J/g473 BTU/lb
Specific Heat Capacity 0.812 J/g-°C0.194 BTU/lb-°F
Melting Point 1205 - 1350 °C2201 - 2460 °F
Solidus 1205 °C2201 °F
Liquidus 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.50 %<= 0.50 %
Carbon, C <= 0.050 %<= 0.050 %
Iron, Fe >= 21.32 %>= 21.32 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 74 - 78 %74 - 78 %
Sulfur, S <= 0.0030 %<= 0.0030 %
Titanium, Ti <= 0.10 %<= 0.10 %
 
Descriptive Properties
Angle of Repose40°-60°
Solubility in alkalisOxidizes with formation of H2 in Alkalis
Solubility in Hydrofluoric AcidSoluble with formation of SiF4
Solubility in Mineral AcidsSoluble with formation of H2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem HP FeSi 75 0.05 Ti High Purity Ferrosilicon
Elkem HP FeSi 75 0.025 Ti High Purity Ferrosilicon
Elkem FeSi 0.10 Al Low Al Ferrosilicon
Elkem FeSi 0.30 Al Low Al Ferrosilicon
Elkem HP FeSi 75 0.02 Ti High Purity Ferrosilicon

NELKEM15 / 16173

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.