MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Edgetek® PI-30GF/000 Polyether Imide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Filler Content 30 %Glass Fiber Reinforcement
Water Absorption 0.18 %
@Thickness 3.18 mm
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 172 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 - 5.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8960 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 221 MPaASTM D790
Flexural Modulus 8960 MPaASTM D790
Izod Impact, Notched 91.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 399 °C
 
Descriptive Properties
FeaturesGeneral Purpose
 High Heat Resistance
FormsPellets
Generic MaterialPEI
Generic NamePolyether Imide (PEI)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 South America
UsesAutomotive Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® PI-30GF/000R BLACK Polyether Imide (PEI)
Avient Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI)
Ensinger Sintimid™ V Unfilled Polyimide (PI)
LATI Latamid 12 CP/85 PA 12
LATI Latigray 82-02 CX/80 PA 12

PH0POL0005 / 144574

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.