MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGY VeTron® Glass Fiber
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Launched 2002, for Vinyl Ester and Polyester resins. Binder is VE1 silane for Vinyl Esters. Acid resistant. Moderate alkali resistance.

Information provided by AGY Holding Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/cc
Water Absorption 0.00 %
Loss On Ignition 0.50 %
Filament Diameter 14 - 26 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 4500 MPa
@Temperature 23.0 °C
Elongation at Break 5.5 %
Modulus of Elasticity 86.0 GPa
Poissons Ratio 0.22
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 825 °C
Maximum Service Temperature, Inert 825 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
S-2 Glass® Fiber
AGY ZenTron® S-2 Generic S-Glass Fiber
E-Glass Fiber, Generic
A-Glass Fiber, Generic
S-Glass Fiber, Generic

CGLASS02 / 932

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.