MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem S-711 Silicone Sprays
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: The following silicone sprays are mold release and lubricating agents formulated with high quality silicone polymers dispersed in a quick drying solvent carrier. These clear liquid sprays are available in 411 ml or 530 ml aerosol cans, 12 cans per case. The base silicones formulated in these release systems range in base silicone viscosity, content and modification (for paintable and urethane products). All of these products are CFC free and do not contain 1,1,1 trichloroethane.

Applications: These versatile aerosol products are utilized as release agents in compression, transfer and injection processing of rubber, plastic and urethane articles. Other uses included lubricants to improve slip on coated surfaces, weather stripping and channels and during cutting operations. Specific formulating of these release systems provide key features such as: high water repellency and dielectric strength, colorless, non-staining residue, good thermal stability, fast drying properties and excellent lubricity. The MR (mold release) and 7-Spray grades are general release systems; 7-Spray contains a higher silicone content. S-903 contains a high viscosity base silicone and is used where a thicker coating is required. S-711 and PMR (paintable mold release) are specialty grades in which the base silicone has been modified with a resin or alkyl functionality. S-711 is formulated for cast and skin urethanes and epoxy products. PMR is a paintable mold release formulated for rubber and plastics products that require post finishing.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.975 g/cc0.975 g/cc
Viscosity 500000 cP500000 cPBase Silicone
 
Thermal PropertiesMetricEnglishComments
Flash Point 158 °C316 °FOpen cup
 
Descriptive Properties
Content0.11Silicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH373 / 315291

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.