MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® Care ME71 Medical Grade Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® Care ME71 is free of plasticizers and heat and light stabilized.

Features: High bursting strength; Flexible and reliable; High chemical resistance; Low sliding friction; High toughness; Good mechanical properties; Low processing tolerances.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.013 cm/cmISO 294-4, 2577
Melt Flow 75 g/10 min
@Load 2.16 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 61.0 MPaISO 527
Tensile Strength, Yield 39.0 MPaISO 527
Elongation at Break 420 %Nominal; ISO 527
Elongation at Yield 13 %ISO 527
Tensile Modulus 1090 MPaISO 527
50% Modulus 0.0290 GPa
@Strain 50 %
ISO 527
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 170 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 177 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 111 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CISO 75-1/-2
Vicat Softening Point 137 °CMethod B: 10 N, 50 K/h; ISO 306
 172 °CMethod A: 10 N, 50 K/h; ISO 306
Flammability Test 1.0
@Thickness 1.60 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® X7293 Nylon 12, Extrusion/Tubing Grade
Evonik Vestamid® L2124 Plasticized Nylon 12
Evonik VESTAMID® E62-S1 Nylon 12 Elastomer
Evonik VESTAMID® DX9303 Nylon 612
Evonik VESTAMID® Care ML94 Medical Grade Nylon 12

PEVONIK819 / 243028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.