MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon™ 640XT X Fine Powder PTFE Resin for Paste Extrusion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded

Material Notes: Teflon™ PTFE 640XT X is a polytetrafluoroethylene fine powder resin used primarily for paste extrusion. Teflon™ PTFE 640XT X offers the excellent combination of properties typical of Teflon™ fluoroplastic resins. Teflon™ PTFE 640XT X is designed for processing over a wide extrusion reduction ratio range (250:1–5000:1), with excellent performance even at the top of this range. Due to its outstanding transformation characteristics, Teflon™ PTFE 640XT X can be extruded with very low lubricant levels over a wide reduction ratio range, while the extrusion pressure remains low. For example, Teflon™ PTFE 640XT X can be extruded into wire with excellent performance in the reduction ratio range of 1000:1–4500:1 with a single lubricant level of 16% (based on total weight). This means that a single PTFE/ lubricant mixture can be used for many constructions being manufactured in the same size extruder line. Teflon™ PTFE 640XT X is mainly used for insulation of high performance wire and cables, as well as tubing. It is also suitable for other typical applications, such as additives where some properties of PTFE are required.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.159 g/ccASTM D4895
Bulk Density 0.525 g/ccASTM D4895
Water Absorption <= 0.010 %
@Time 86400 sec
ASTM D570
Particle Size 450 µmAverage; ASTM D4895
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50 - 65ASTM D2240
Tensile Strength 28.0 MPaASTM D1457
Elongation at Break 400 %ASTM D1457
Flexural Modulus 0.496 GPaASTM D790
Flex Crack Resistance >= 1.00e+6Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched 3.50 ft-lb/inASTM D256
Coefficient of Friction 0.050 - 0.10ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+18 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 0.100 mm
ASTM D149
Dissipation Factor <= 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 326 °CSecond Peak; ASTM D4591
 327 °CASTM D3418
 344 °CInitial Peak; ASTM D4591
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Detergent Resistance (hours)24On grit blast aluminum
 264
 624On aluminum
Extrusion Pressure (MPa)22ASTM D4895. @ RR= 1600:1
 28ASTM D4895. @ RR= 2500:1
Heat of Combustion5.1 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)192ASTM B117. 5% NaCl at 35 °C (95 °F). On aluminum.
 744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Thermal Instability Index=15ASTM D4895
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8824 / 268750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.