MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Freudenberg Sealing Technologies 80 EPDM 185713 Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: EPDM enjoys high acceptance in the food and pharmaceutical industries. EPDM is indispensable for CIP (clean in place) or SIP (sterilization in place) cleaning processes. However, the fat content of the media may not exceed certain limits. EPDM is a polymerization made of ethylene, propylene and a diene monomer.

It displays high media resistance to brake fluids, acids and lyes, the flame-resistant hydraulic fluids HFC and HFD, hot water and steam. But it is not stable in petroleum-based oils and fats or in gasoline and hydrocarbons. In turn, this material is inexpensive and can be used almost universally – although not with oils.

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282DIN ISO 7619-1
Tensile Strength 18.8 MPa2730 psiDIN 53504, S2
Elongation at Break 170 %170 %DIN 53504, S2
100% Modulus 9.30 MPa1350 psiDIN 53504, S2
Rebound 48 %48 %DIN 53512
Tear Strength 16.4 kN/m93.6 pliDIN 53515
Compression Set  16 %
@Temperature 150 °C,
Time 79200 sec
16 %
@Temperature 302 °F,
Time 22.0 hour
DIN ISO 815
 36 %
@Temperature 120 °C,
Time 79200 sec
36 %
@Temperature 248 °F,
Time 22.0 hour
P-VW 3307
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -15.0 °C5.00 °F
 
Descriptive Properties
Colorblack
Cross-linkingperoxidic
Microhardness (IRHD)82DIN ISO 48 Procedure M

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9169 / 293690

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.