MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tabriz GPPS 1810 Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: GPPS1810 is an easy flowing crystal polystyrene designed for injection applications. Applications: Petri dishes, blood sample tubes, disposable beakers, thin wall moldings.

Information provided by Tabriz Petrochemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 200 °C
20 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7070ASTM D785
Tensile Strength at Break 40.0 MPa5800 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 4.15 GPa602 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °F50°C/hr 1kg; ASTM D1525
 
Descriptive Properties
Styrene Residual Monomer<500 ppmCLG LABPSG004 (Atofina Test)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1810/1811 Polystyrene
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
Videolar-Innova 500 Crystal Polystyrene (GPPS)
Total PSC 1960N Crystal Polystyrene
SYNTHOS Krasten® 137 General Purpose Polystyrene

PTABRZ933 / 198239

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.