MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ovako 11SMn30, Green Cut 2715 Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Green Cut steel has been developed to replace leaded free-cutting steels, when the customer is looking for an environmentally friendly alternative. High sulfur content combined with M-treatment gives superior machinability both with carbide and HSS tools.

M-SteelThe concept: Our M-Steel treatment can be applied to any steel grade. The basis for the concept is that non-metallic inclusions are modified and controlled with calcium treatment. These inclusions are modified in a way to maximize machinability and to improve transverse fatigue strength. In this way, a protective layer is formed on the cutting tool during machining that very significantly reduces the wear on the tool and increases the tool life. At every stage of the M-Steel production process the material is optimised to improve machinability, from raw material through melt, to casting, hot rolling and the final heat treatment. Individual delivery requirements can be met to supply your material in the best form for your machines in compliance with tight straightness and dimensional tolerances. M-Steel has a consistent machinability from cast to cast, meaning that machines can be run with fixed high cutting rates and predictable tool change intervals from one production run to another. Recent findings also show that the MSteel effect is particularly pronounced in turning in very hard condition using Cubic Boron Nitride (CBN) inserts. Replacing traditional grinding of case- or induction-hardened surfaces with Hard Part Turning can mean very large cost savings, together with production lead time and quality improvements.

Information provided by Ovako

Key Words: SS 1912, SS 1914
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120 - 160
@Thickness 25.0 - 200 mm
120 - 160
@Thickness 0.984 - 7.87 in
Tensile Strength 350 - 540 MPa
@Thickness 25.0 - 200 mm
50800 - 78300 psi
@Thickness 0.984 - 7.87 in
Tensile Strength, Yield >= 270 MPa
@Thickness 25.0 - 200 mm
>= 39200 psi
@Thickness 0.984 - 7.87 in
Elongation at Break 22 %
@Thickness 25.0 - 200 mm
22 %
@Thickness 0.984 - 7.87 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 436 °C817 °FMS
 715 °C1320 °FAC1
 843 °C1550 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 - 0.14 %0.050 - 0.14 %
Iron, Fe 97.68 - 98.68 %97.68 - 98.68 %As Balance
Manganese, Mn 1.0 - 1.4 %1.0 - 1.4 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 0.050 - 0.40 %0.050 - 0.40 %
Sulfur, S 0.22 - 0.33 %0.22 - 0.33 %
 
Descriptive Properties
WeldabilityCEV 0.4max
 Pcm 0.22max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Ovako 11SMn30, Green Cut 2715 Steel, +C
ATI Allvac® VascoMax® T-200 Specialty Steel
AK Steel 316 Austenitic Stainless steel
316 Stainless Steel, annealed sheet

NOVAKO062 / 234361

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.