MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Universal Wire Works 117 Nickel Alloy Welding Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Alloy 117 is a nickel alloy electrode for welding nickel-chromium-cobalt-molybdenum alloys (UNS # N06617). This alloy electrode provides optimum strength and oxidation resistance above 1500 degrees F up to 2100 degrees F, especially when welding base metals of nickel-iron-chromium composition. Alloy 117 can also be used for overlay cladding where similar alloy is required.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS A5.11 Class ENiCrCoMo-1; ASME SFA-5.11 Class ENiCrCoMo-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.8 MPa11000 psi
Tensile Strength, Yield 600 MPa87000 psi
Elongation at Break 26 %26 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1150 °C2100 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.65 %0.65 %
Carbon, C 0.060 %0.060 %
Chromium, Cr 21.65 %21.65 %
Cobalt, Co 11.85 %11.85 %
Iron, Fe 1.5 %1.5 %
Manganese, Mn 0.45 %0.45 %
Molybdenum, Mo 8.8 %8.8 %
Nickel, Ni 54.6 %54.6 %As Remainder
Phosphorus, P 0.012 %0.012 %
Silicon, Si 0.35 %0.35 %
Sulfur, S 0.0050 %0.0050 %
Titanium, Ti 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee MHC Molybdenum-Hafnium-Carbon Rod
Overview of materials for Refractory Metal
Overview of materials for Molybdenum Alloy

NUWW122 / 19647

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.