MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C51190, H04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Excellent Suitability – Soldering, Brazing, Butt Weld; Good Suitability – Gas Shielded Arc Welding, Spot Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 215
@Load 0.500 kg
215
@Load 1.10 lb
Tensile Strength 648 MPa94000 psi
Tensile Strength, Yield 634 MPa92000 psi0.2% Offset
Elongation at Break 11 %11 %
Tensile Modulus 79.3 GPa11500 ksi
Fatigue Strength 269 MPa
@# of Cycles 1.00e+8
39000 psi
@# of Cycles 1.00e+8
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000780 ohm-cm0.00000780 ohm-cm22% IACS
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 7.67 W/m-K53.2 BTU-in/hr-ft²-°F
Melting Point 950.0 - 1053 °C1742 - 1927 °F
Solidus 950.0 °C1742 °F
Liquidus 1053 °C1927 °F
Annealing Point >= 450 °C>= 842 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 273 °C>= 523 °FStress Relief
Hot-Working Temperature 800.0 - 950.0 °C1472 - 1742 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co <= 0.15 %<= 0.15 %
Copper, Cu 93.1 - 96.9 %93.1 - 96.9 %As Balance
Iron, Fe 0.050 - 0.15 %0.050 - 0.15 %
Lead, Pb <= 0.020 %<= 0.020 %
Phosphorus, P 0.025 - 0.045 %0.025 - 0.045 %
Tin, Sn 3.0 - 6.5 %3.0 - 6.5 %
 
Descriptive Properties
Proportional Limit87 ksi
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC51190x3 / 292138

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.