Pro-fax HP403G is a general purpose homopolymer with good heat resistance and high tensile strength. It is available in pellet form, and it is typically used in extrusion applications. Applications: General Sheet Extrusion, Nets, Strapping, Thermoformed Food ContainersInformation provided by LyondellBasell. |