MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Verde Fuoco Metasomatite Architectural Stone
Categories: Ceramic

Material Notes: Verde Fuoco ('Green Fire' in Italian; also called Harlequin) takes its name from the vivid green and red colors that dominate its varied appearance. It is a premium grade stone, used in applications such as countertops and floor tiles. Although commonly called granite in the architectural industry, it is probably of a granitic composition with the usual feldspar, quartz and ferromagnesian minerals which has undergone extensive metamorphism /metasomatism – not quite to gneissic grade- and alteration due to hydrothermal processes. To that effect, many minerals have been formed in the process including hornblende, chlorite, epidote, carbonates, iron, a variety of hydrothermal clays and silicification. The unique colors of the rock resulted from the mixing and reactions of these minerals and the stressing and straining shaped the patterns that are seen in the rock. Verde Fuoco / Harlequin also hosts fine disseminated sulfides including pyrite and possibly chalcopyrite grains and occasional micro veinlets. It is quarried in Gawler Craton of South Australia.

Information provided by Stone Boutique Australia.

Key Words: Granite
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.90 - 3.30 g/cc0.105 - 0.119 lb/in³
Water Absorption 0.16 %0.16 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 18.7 MPa2710 psidry
 23.6 MPa3420 psisoaked
Compressive Strength 206.3 MPa29920 psidry
 218 MPa31600 psisoaked
 
Descriptive Properties
Mineralogy1.6%Carbonate & other minerals
 11.2%Amphibole
 19.2%Plagioclase
 33.5%Pyroxene
 34.5%Epidote

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Granite
Raschig Group PiMC 1949 Granite colors
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Marl
Soapstone

BMIN900 / 191527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.