MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Lupolen 2221F LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lupolen 2221F is a fractional melt index homopolymer LDPE resin designed for film applications requiring an excellent balance of clarity, stiffness, shrink and strength. 2221F is selected by customers for collation shrink films, pallet shrink films, packaging films and heavy duty films where clarity and stiffness are important. 2221F contains an antioxidant.

Availability: Africa-Middle East; Asia-Pacific

Application: Bags & Pouches; Clarity Film; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Industrial Film; Lamination Film; Shrink Film; Surface Protection Film

Market: Flexible Packaging

Processing Method: Blown Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 0.800 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.800 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiASTM D882
Film Elongation at Break, MD 400 %400 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Secant Modulus, MD 0.220 GPa31.9 ksi1% Modulus; ASTM D882
Secant Modulus, TD 0.250 GPa36.3 ksi1% Modulus; ASTM D882
Elmendorf Tear Strength MD 270 g270 gASTM D1922
Elmendorf Tear Strength TD 290 g290 gASTM D1922
Dart Drop Test 150 g0.331 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 25.0 MPa3630 psiASTM D882
Film Tensile Strength at Break, TD 21.0 MPa3050 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze <= 6.50 %<= 6.50 %ASTM D1003
Gloss >= 72.0 %>= 72.0 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9649 / 324584

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.