MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Universal Wire Works Haynes 25 (L-605) (AMS 5796) Filler Metal
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Haynes Alloy 25 (L-605) can be welded using the gas tungsten arc, gas metal arc and plasma arc processes. Alloy 25 has good resistance to corrosion and is resistant to oxidation and carburization to 1900°F. This alloy has been used extensively in jet engine parts including turbine blades, combustion chambers, turbine rings and afterburner parts.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 20 %
Cobalt, Co >= 49.3 %As Remainder
Iron, Fe <= 3.0 %
Manganese, Mn 1.5 %
Nickel, Ni 10 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %
Tungsten, W 15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes 25 alloy, sheet
Haynes 25 alloy, room temperature after 0% cold reduction
AISI 1215 Steel, cold drawn, 19-38 mm round
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet
ATI Allvac® Nickelvac® L-605 Cobalt-Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal

NUWW306 / 19739

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.