MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Anderman Ceramics EC70P Mullite-Bonded Porous Silicon Carbide (70%)
Categories: Ceramic; Carbide

Material Notes: Excellent thermal shock properties when in contact with molten metal. Available as tube, sheath, or rod up to 7.2 ft (2.2 m) long with diameters 0.6" to 4.7".

Information provided by Anderman Ceramics.

Key Words: SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/cc
Open Porosity 25 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 7.00 W/m-K
@Temperature 20.0 - 100 °C
Maximum Service Temperature, Air 1400 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 19 %
SiC 70 %
SiO2 10.5 %
 
Descriptive Properties
Thermal Shock ResistanceVery Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)
Silicon Carbide, CVD
Silicon Carbide, sublimed
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber

CANDER05 / 478

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.