MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Categories: Ceramic; Glass; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situations. Many of the advantages from the use of Fillite, including increased filler loading and improved rheology, are directly attributed to the spherical nature of the material.

Typical Applications
SGHA has a higher alumina content than the normal Fillite grades and has been specifically developed for higher temperature applications such as refractories, foundry applications, high temperature resistant coatings. Other higher alumina grades are whiter in color and particularly suitable for gypsum board jointing compounds, veneering plasters, stuccos, sealants, coatings and cast resins.

Advantages
Reduced weight, increased filler loadings, better flow characteristics, less shrinkage and warping. Improved physical properties in moldings, castings, and laminates, reduced water absorption, improved flame retardance, improved chemical resistance.

All information provided by Fillite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 - 0.480 g/cc0.0145 - 0.0173 lb/in³
Pellet Density 0.700 - 0.900 g/cc0.0253 - 0.0325 lb/in³
Loss On Ignition <= 2.0 %<= 2.0 %
Particle Size 5.0 - 180 µm5.0 - 180 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.05.0
Compressive Strength 13.8 - 27.6 MPa2000 - 4000 psiCrush Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.110 W/m-K0.763 BTU-in/hr-ft²-°F
Melting Point 1400 °C2550 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.30 %<= 0.30 %Surface
 
Component Elements PropertiesMetricEnglishComments
Al2O3 <= 39 %<= 39 %
CO2 70 %70 %
Fe2O3 <= 2.0 %<= 2.0 %
Nitrogen, N 30 %30 %
SiO2 55 - 65 %55 - 65 %
 
Descriptive Properties
Average Wall Thickness (% Sphere Diameter)5-10
ColorOff-White
Packing Factor (%)60-65
Particle Size Distribution (%)100% Passing 500 microns
 100% Passing 300 microns
 10-20% Passing 50 microns
 30-60% Passing 100 microns
 99.5-100% Passing 180 microns

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Foam
3M K20 Glass Bubbles
3M K15 Glass Bubbles
3M K1 Glass Bubbles
3M S22 Glass Bubbles

PTRELL204 / 83962

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.