MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Network Polymers MS 600 Styrene Methyl Methacrylate Copolymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Polystyrene (PS); Styrene/Methyl Methacrylate Copolymer (SMMA)

Material Notes: Description: Styrene Methyl Methacrylate Copolymer

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Water Absorption 0.10 %24 hours; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D955
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength, Yield 10000 psi2 in per min; ASTM D638
Elongation at Break 5.5 %chs 2 in/min; ASTM D638
Modulus of Elasticity 3.169 GPaASTM D638
Izod Impact, Notched 0.400 ft-lb/in0.125 inch bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °FASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer
Arkema Altuglas® 84 L Acrylic-Styrene Copolymer
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
INEOS Styrolution NAS® 21 Styrene Methyl Methacrylate (SMMA)
A. Schulman Diamond MS-170 Styrene Methyl Methacrylate Terpolymer

PDIAM046 / 29884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.